Grooving and parting insert, groove width 8.1 mm, grade TN30
PTNT08TN30
Parameters
- Groove width
- 8.1 mm
- Grade
- TN30
Source: Canela Parting and Grooving, page B08.
More parameters 4
- Use
- Grooving and parting
- Use
- parting, external grooving
- Workpiece materials (ISO)
- P, M, K
- Insert series
- PTNT
Some values are worked out from the printed ones.
Other sizes of the series 19
| Code | Groove width, mm | Grade |
|---|---|---|
| PTNT02PM25 | 2.1 | PM25 |
| PTNT02PM40 | 2.1 | PM40 |
| PTNT02TN30 | 2.1 | TN30 |
| PTNT03KM15 | 3.1 | KM15 |
| PTNT03PM25 | 3.1 | PM25 |
| PTNT03PM40 | 3.1 | PM40 |
| PTNT03TIN21 | 3.1 | TIN21 |
| PTNT03TN30 | 3.1 | TN30 |
| PTNT04PM25 | 4.1 | PM25 |
| PTNT04PM40 | 4.1 | PM40 |
| PTNT04TIN21 | 4.1 | TIN21 |
| PTNT04TN30 | 4.1 | TN30 |
| PTNT05KM15 | 5.1 | KM15 |
| PTNT05PM25 | 5.1 | PM25 |
| PTNT05TN30 | 5.1 | TN30 |
| PTNT06TN30 | 6.1 | TN30 |
| PTNT08TN30 | 8.1 | TN30 |
| PTNT09PM25 | 9.1 | PM25 |
| PTNT09TN30 | 9.1 | TN30 |
Cutting data
As the manufacturer prints them. The site works nothing out. Canela, Canela Parting and Grooving, p. B19, B56, B58, B60.
Grooving and parting /Segat i ranurat | B
The manufacturer's recommended cutting data for this item
Recommended cutting conditions / Condicions de tall recomanades
| Cutting speed m/min. / Velocitat de tall m/min. | |
|---|---|
| TN30 | |
| P | 60-200 |
| M | 60-180 |
| K | 60-150 |
| S | 20-50 |
| P | 60-200 |
| M | 60-180 |
| K | 60-150 |
| S | 20-50 |
| P | 60-200 |
| M | 60-180 |
| K | 60-150 |
| S | 20-50 |
Notes: - Partial profile 55º. - Partial profile 60º. - Perfil parcial 55º. - Perfil parcial 60º. - Maximum deep of cut is 3,00 mm. - Too low cutting speed will result in inadequate tool life and it is advisable - Profunditat de tall màxima: 3,00 mm. - Una velocitat de tall massa baixa donarà com a resultat una durada
Open the catalog page. The table is marked on the page. The manufacturer's recommended cutting data for this item
Nominal cutting speed for parting
| P | ||
|---|---|---|
| Basic grades | Specific cutting force | |
| TN30 | N/mm² | |
| Cutting speed m/min. | ||
| P · Unalloyed steel · HB 125 · C=0.15% | 200-150 | 1900 |
| P · Unalloyed steel · HB 150 · C=0.35% | 190-140 | 2100 |
| P · Unalloyed steel · HB 200 · C=0.60% | 170-120 | 2250 |
| P · Low alloyed steel · HB 180 · Annealed | 180-130 | 2100 |
| P · Low alloyed steel · HB 275 · Hardened | 160-110 | 2600 |
| P · Low alloyed steel · HB 300 · Hardened | 150-100 | 2700 |
| P · Low alloyed steel · HB 350 · Hardened | 140-90 | 2850 |
| P · High alloyed steel · HB 200 · Annealed | 110-90 | 2600 |
| P · High alloyed steel · HB 325 · Hardened | 70-50 | 3900 |
| P · Stainless steel · HB 200 · Martensitic / ferritic | 170-120 | 2300 |
| P · Steel · HB 180 · Unalloyed | 130-90 | 2000 |
| P · Steel · HB 200 · Low alloyed | 115-75 | 2500 |
| P · Steel · HB 225 · High alloyed | 100-60 | 2700 |
| M | ||
| M · Stainless steel annealed · HB 180 | 170-120 | 2450 |
| M · Heat-resistant alloys · HB 200 · Annealed Iron base | 3000 | |
| M · Heat-resistant alloys · HB 280 · Aged | 3050 | |
| M · Heat-resistant alloys · HB 250 · Annealed Ni or | 3500 | |
| M · Heat-resistant alloys · HB 350 · Aged Co base | 4150 | |
| M · Heat-resistant alloys · HB 320 · Cast | 4150 | |
| M · Titanium alloys · HB 400 · Ti | 1520 | |
| M · Titanium alloys · HB 950 · Cast a, almost a and a+b | 1675 | |
| M · Titanium alloys · HB 1050 · Aged cast a+b | 1690 | |
| K | ||
| Basic grades | Specific cutting force | |
| TN30 | N/mm² | |
| Cutting speed m/min. | ||
| K · Hardened steel · HB 220 · Hardened steel | 4500 | |
| K · Hardened steel · HB 250 · Manganese steel 12% | 4500 | |
| K · Malleable cast iron · HB 130 · Ferritic | 140-110 | 1100 |
| K · Malleable cast iron · HB 230 · Pearlitic | 100-70 | 1100 |
| K · Cast iron · HB 180 · Low tensile strength | 110-85 | 1100 |
| K · Cast iron · HB 260 · High tensile strength | 100-70 | 1500 |
| K · Nodular SG iron · HB 160 · Ferritic | 100-70 | 1100 |
| K · Nodular SG iron · HB 250 · Pearlitic | 85-60 | 1800 |
| K · Aluminium alloys · HB 60 · Non heat treatable | 1500 | 500 |
| K · Aluminium alloys · HB 100 · Heat treatable | 500 | 800 |
| K · Aluminium alloys (cast) · HB 75 · Non heat treatable | 1500 | 750 |
| K · Aluminium alloys (cast) · HB 90 · Heat treatable | 750 | 900 |
| K · Bronze-brass alloys · HB 110 · Lead alloys, Pb>1% | 300 | 700 |
| K · Bronze-brass alloys · HB 90 · Brass, red brass | 200 | 750 |
| K · Bronze-brass alloys · HB 100 · Bronze and lead-free copper | 150 | 1750 |
Open the catalog page. The table is marked on the page. The manufacturer's recommended cutting data for this item
Nominal cutting speed for grooving
| P | |||
|---|---|---|---|
| External | Internal | Specific cutting force | |
| TN30 | TN30 | N/mm² | |
| Cutting speed m/min. | |||
| P · Unalloyed steel · HB 125 · C=0.15% | 200-150 | 140-105 | 1900 |
| P · Unalloyed steel · HB 150 · C=0.35% | 190-140 | 135-100 | 2100 |
| P · Unalloyed steel · HB 200 · C=0.60% | 170-120 | 120-85 | 2250 |
| P · Low alloyed steel · HB 180 · Annealed | 180-130 | 125-90 | 2100 |
| P · Low alloyed steel · HB 275 · Hardened | 160-110 | 110-80 | 2600 |
| P · Low alloyed steel · HB 300 · Hardened | 150-100 | 105-70 | 2700 |
| P · Low alloyed steel · HB 350 · Hardened | 140-90 | 100-60 | 2850 |
| P · High alloyed steel · HB 200 · Annealed | 110-90 | 80-60 | 2600 |
| P · High alloyed steel · HB 325 · Hardened | 70-50 | 80-35 | 3900 |
| P · Stainless steel · HB 200 · Martensitic / ferritic | 170-120 | 120-85 | 2300 |
| P · Steel · HB 180 · Unalloyed | 130-90 | 90-60 | 2000 |
| P · Steel · HB 200 · Low alloyed | 115-75 | 80-50 | 2500 |
| P · Steel · HB 225 · High alloyed | 100-60 | 70-45 | 2700 |
| M | |||
| External | Internal | Specific cutting force | |
| TN30 | TN30 | N/mm² | |
| M · Stainless steel annealed · HB 180 | 170-120 | 120-85 | 2450 |
| M · Heat-resistant alloys · HB 200 · Annealed Iron base | 3000 | ||
| M · Heat-resistant alloys · HB 280 · Aged | 3050 | ||
| M · Heat-resistant alloys · HB 250 · Annealed Ni or | 3500 | ||
| M · Heat-resistant alloys · HB 350 · Aged Co base | 4150 | ||
| M · Heat-resistant alloys · HB 320 · Cast | 4150 | ||
| M · Titanium alloys · HB 400 | 1520 | ||
| M · Titanium alloys · HB 950 | 1675 | ||
| M · Titanium alloys · HB 1050 | 1690 | ||
| K | |||
| External | Internal | Specific cutting force | |
| TN30 | TN30 | N/mm² | |
| K · Hardened steel · HB 220 · Hardened steel | 4500 | ||
| K · Hardened steel · HB 250 · Manganese steel 12% | 4500 | ||
| K · Malleable cast iron · HB 130 · Ferritic | 140-110 | 100-80 | 1100 |
| K · Malleable cast iron · HB 230 · Pearlitic | 100-70 | 70-50 | 1100 |
| K · Cast iron · HB 180 · Low tensile strength | 110-85 | 80-60 | 1100 |
| K · Cast iron · HB 260 · High tensile strength | 100-70 | 70-50 | 1500 |
| K · Nodular SG iron · HB 160 · Ferritic | 100-70 | 70-50 | 1100 |
| K · Nodular SG iron · HB 250 · Pearlitic | 85-60 | 60-45 | 1800 |
| K · Aluminium alloys · HB 60 · Non heat treatable | 1500 | 1050 | 500 |
| K · Aluminium alloys · HB 100 · Heat treatable | 500 | 350 | 800 |
| K · Aluminium alloys (cast) · HB 75 · Non heat treatable | 1500 | 1050 | 750 |
| K · Aluminium alloys (cast) · HB 90 · Heat treatable | 750 | 525 | 900 |
| K · Bronze-brass alloys · HB 110 | 300 | 210 | 700 |
| K · Bronze-brass alloys · HB 90 | 200 | 140 | 750 |
| K · Bronze-brass alloys · HB 100 | 150 | 105 | 1750 |
Open the catalog page. The table is marked on the page. The manufacturer's recommended cutting data for this item
Nominal cutting speed for profiling
| P | ||
|---|---|---|
| Basic grades | Specific cutting force | |
| TN30 | N/mm² | |
| Cutting speed m/min. | ||
| P · Unalloyed steel · HB 125 · C=0.15% | 200 | 1900 |
| P · Unalloyed steel · HB 150 · C=0.35% | 190 | 2100 |
| P · Unalloyed steel · HB 200 · C=0.60% | 170 | 2250 |
| P · Low alloyed steel · HB 180 · Annealed | 180 | 2100 |
| P · Low alloyed steel · HB 275 · Hardened | 160 | 2600 |
| P · Low alloyed steel · HB 300 · Hardened | 150 | 2700 |
| P · Low alloyed steel · HB 350 · Hardened | 140 | 2850 |
| P · High alloyed steel · HB 200 · Annealed | 130 | 2600 |
| P · High alloyed steel · HB 325 · Hardened | 100 | 3900 |
| P · Stainless steel · HB 200 · Martensitic / ferritic | 170 | 2300 |
| P · Steel · HB 180 · Unalloyed | 130 | 2000 |
| P · Steel · HB 200 · Low alloyed | 115 | 2500 |
| P · Steel · HB 225 · High alloyed | 100 | 2700 |
| M | ||
| M · Stainless steel annealed · HB 180 | 170 | 2450 |
| M · Heat-resistant alloys · HB 200 · Annealed Iron base | 3000 | |
| M · Heat-resistant alloys · HB 280 · Aged | 3050 | |
| M · Heat-resistant alloys · HB 250 · Annealed Ni or | 3500 | |
| M · Heat-resistant alloys · HB 350 · Aged Co base | 4150 | |
| M · Heat-resistant alloys · HB 320 · Cast | 4150 | |
| M · Titanium alloys · HB 400 · Ti | 1520 | |
| M · Titanium alloys · HB 950 · Cast a, almost a and a+b | 1675 | |
| M · Titanium alloys · HB 1050 · Aged cast a+b | 1690 | |
| K | ||
| Basic grades | Specific cutting force | |
| TN30 | N/mm² | |
| Cutting speed m/min. | ||
| K · Hardened steel · HB 220 · Hardened steel | 4500 | |
| K · Hardened steel · HB 250 · Manganese steel 12% | 4500 | |
| K · Malleable cast iron · HB 130 · Ferritic | 140 | 1100 |
| K · Malleable cast iron · HB 230 · Pearlitic | 110 | 1100 |
| K · Cast iron · HB 180 · Low tensile strength | 110 | 1100 |
| K · Cast iron · HB 260 · High tensile strength | 100 | 1500 |
| K · Nodular SG iron · HB 160 · Ferritic | 100 | 1100 |
| K · Nodular SG iron · HB 250 · Pearlitic | 85 | 1800 |
| K · Aluminium alloys · HB 60 · Non heat treatable | 1500 | 500 |
| K · Aluminium alloys · HB 100 · Heat treatable | 500 | 800 |
| K · Aluminium alloys (cast) · HB 75 · Non heat treatable | 1500 | 750 |
| K · Aluminium alloys (cast) · HB 90 · Heat treatable | 750 | 900 |
| K · Bronze-brass alloys · HB 110 · Lead alloys, Pb>1% | 300 | 700 |
| K · Bronze-brass alloys · HB 90 · Brass, red brass | 200 | 750 |
| K · Bronze-brass alloys · HB 100 · Bronze and lead-free copper | 150 | 1750 |
Open the catalog page. The table is marked on the page. We reply with price and delivery time.