Grooving and parting insert, r 0.2 mm, grade TL40
MRCN2.2TL40
Parameters
- rCorner radius
- 0.2 mm
- Groove width
- 2.2 mm
- Grade
- TL40
Source: Canela Parting and Grooving, page B08. Symbols as the catalog table prints them.
More parameters 5
- Holder system
- Canela CZCB
- Use
- Grooving and parting
- Use
- parting, external grooving
- Workpiece materials (ISO)
- P, M
- Insert series
- MRCN
Some values are worked out from the printed ones.
Other sizes of the series 6
| Code | r, mm | Groove width, mm | Grade |
|---|---|---|---|
| MRCN1.6TL40 | 0.15 | 1.6 | TL40 |
| MRCN2.2TL40 | 0.2 | 2.2 | TL40 |
| MRCN3.0TL40 | 0.2 | 3 | TL40 |
| MRCN4.0TL40 | 0.2 | 4 | TL40 |
| MRCN5.0TL40 | 0.3 | 5 | TL40 |
| MRCN6.0TL40 | 0.4 | 6 | TL40 |
Cutting data
As the manufacturer prints them. The site works nothing out. Canela, Canela Parting and Grooving, p. B56, B58, B60.
The manufacturer's recommended cutting data for this item
Nominal cutting speed for parting
| P | ||
|---|---|---|
| TL40 | Specific cutting force | |
| N/mm² | ||
| P · Unalloyed steel · HB 125 · C=0.15% | 160-120 | 1900 |
| P · Unalloyed steel · HB 150 · C=0.35% | 150-110 | 2100 |
| P · Unalloyed steel · HB 200 · C=0.60% | 130-90 | 2250 |
| P · Low alloyed steel · HB 180 · Annealed | 140-100 | 2100 |
| P · Low alloyed steel · HB 275 · Hardened | 120-80 | 2600 |
| P · Low alloyed steel · HB 300 · Hardened | 110-70 | 2700 |
| P · Low alloyed steel · HB 350 · Hardened | 90-60 | 2850 |
| P · High alloyed steel · HB 200 · Annealed | 70-60 | 2600 |
| P · High alloyed steel · HB 325 · Hardened | 45-30 | 3900 |
| P · Stainless steel · HB 200 · Martensitic / ferritic | 130-90 | 2300 |
| P · Steel · HB 180 · Unalloyed | 100-60 | 2000 |
| P · Steel · HB 200 · Low alloyed | 90-50 | 2500 |
| P · Steel · HB 225 · High alloyed | 80-40 | 2700 |
| M | ||
| M · Stainless steel annealed · HB 180 | 130-90 | 2450 |
| M · Heat-resistant alloys · HB 200 · Annealed Iron base | 3000 | |
| M · Heat-resistant alloys · HB 280 · Aged | 3050 | |
| M · Heat-resistant alloys · HB 250 · Annealed Ni or | 3500 | |
| M · Heat-resistant alloys · HB 350 · Aged Co base | 4150 | |
| M · Heat-resistant alloys · HB 320 · Cast | 4150 | |
| M · Titanium alloys · HB 400 · Ti | 1520 | |
| M · Titanium alloys · HB 950 · Cast a, almost a and a+b | 1675 | |
| M · Titanium alloys · HB 1050 · Aged cast a+b | 1690 | |
Open the catalog page. The table is marked on the page. The manufacturer's recommended cutting data for this item
Nominal cutting speed for grooving
| P | |||
|---|---|---|---|
| TL40 | Specific cutting force | ||
| Cutting speed m/min. | N/mm² | ||
| P · Unalloyed steel · HB 125 · C=0.15% | 160-120 | 110-85 | 1900 |
| P · Unalloyed steel · HB 150 · C=0.35% | 150-110 | 105-80 | 2100 |
| P · Unalloyed steel · HB 200 · C=0.60% | 130-90 | 90-60 | 2250 |
| P · Low alloyed steel · HB 180 · Annealed | 140-100 | 100-70 | 2100 |
| P · Low alloyed steel · HB 275 · Hardened | 120-80 | 85-55 | 2600 |
| P · Low alloyed steel · HB 300 · Hardened | 110-70 | 80-50 | 2700 |
| P · Low alloyed steel · HB 350 · Hardened | 90-60 | 60-45 | 2850 |
| P · High alloyed steel · HB 200 · Annealed | 70-60 | 50-45 | 2600 |
| P · High alloyed steel · HB 325 · Hardened | 45-30 | 32-20 | 3900 |
| P · Stainless steel · HB 200 · Martensitic / ferritic | 130-90 | 90-60 | 2300 |
| P · Steel · HB 180 · Unalloyed | 100-60 | 70-45 | 2000 |
| P · Steel · HB 200 · Low alloyed | 90-50 | 60-35 | 2500 |
| P · Steel · HB 225 · High alloyed | 80-40 | 55-30 | 2700 |
| M | |||
| TL40 | Specific cutting force | ||
| Cutting speed m/min. | N/mm² | ||
| M · Stainless steel annealed · HB 180 | 130-90 | 90-60 | 2450 |
| M · Heat-resistant alloys · HB 200 · Annealed Iron base | 3000 | ||
| M · Heat-resistant alloys · HB 280 · Aged | 3050 | ||
| M · Heat-resistant alloys · HB 250 · Annealed Ni or | 3500 | ||
| M · Heat-resistant alloys · HB 350 · Aged Co base | 4150 | ||
| M · Heat-resistant alloys · HB 320 · Cast | 4150 | ||
| M · Titanium alloys · HB 400 | 1520 | ||
| M · Titanium alloys · HB 950 | 1675 | ||
| M · Titanium alloys · HB 1050 | 1690 | ||
Open the catalog page. The table is marked on the page. The manufacturer's recommended cutting data for this item
Nominal cutting speed for profiling
| P | ||
|---|---|---|
| TL40 | Specific cutting force | |
| N/mm² | ||
| P · Unalloyed steel · HB 125 · C=0.15% | 160 | 1900 |
| P · Unalloyed steel · HB 150 · C=0.35% | 150 | 2100 |
| P · Unalloyed steel · HB 200 · C=0.60% | 130 | 2250 |
| P · Low alloyed steel · HB 180 · Annealed | 140 | 2100 |
| P · Low alloyed steel · HB 275 · Hardened | 120 | 2600 |
| P · Low alloyed steel · HB 300 · Hardened | 110 | 2700 |
| P · Low alloyed steel · HB 350 · Hardened | 90 | 2850 |
| P · High alloyed steel · HB 200 · Annealed | 100 | 2600 |
| P · High alloyed steel · HB 325 · Hardened | 60 | 3900 |
| P · Stainless steel · HB 200 · Martensitic / ferritic | 130 | 2300 |
| P · Steel · HB 180 · Unalloyed | 100 | 2000 |
| P · Steel · HB 200 · Low alloyed | 90 | 2500 |
| P · Steel · HB 225 · High alloyed | 70 | 2700 |
| M | ||
| M · Stainless steel annealed · HB 180 | 120 | 2450 |
| M · Heat-resistant alloys · HB 200 · Annealed Iron base | 3000 | |
| M · Heat-resistant alloys · HB 280 · Aged | 3050 | |
| M · Heat-resistant alloys · HB 250 · Annealed Ni or | 3500 | |
| M · Heat-resistant alloys · HB 350 · Aged Co base | 4150 | |
| M · Heat-resistant alloys · HB 320 · Cast | 4150 | |
| M · Titanium alloys · HB 400 · Ti | 1520 | |
| M · Titanium alloys · HB 950 · Cast a, almost a and a+b | 1675 | |
| M · Titanium alloys · HB 1050 · Aged cast a+b | 1690 | |
Open the catalog page. The table is marked on the page. Open the price request
We reply with price and delivery time.
Delta analogs
No direct or close analog was found among the Delta brands.